Yayın: THE RETENTION DIAGRAM OF POLY(P-CHLOROSTYRENE) AND TERT-BUTYL ACETATE BY THE INVERSE GAS-CHROMATOGRAPHY METHOD
| dc.contributor.author | CANKURTARAN, O | |
| dc.contributor.author | YILMAZ, F | |
| dc.contributor.institutionauthor | YILMAZ, Ayçe Feride | |
| dc.contributor.institutionauthor | CANKURTARAN, Özlem | |
| dc.date.accessioned | 2026-06-27T12:56:39Z | |
| dc.date.issued | 1993 | |
| dc.description.abstract | The retention diagram of poly(p-chlorostyrene) for tert-butyl acetate was obtained by the inverse gas chromatograhy method. This polymer-solvent pair exhibits a lower critical solution temperature, i.e., the solubility of the polymer in the solvent decreases with temperature. The obtained retention diagram of this polymer-solvent system contained an extra region with a negative slope at temperatures lower than 90-degrees-C. It appears that in this region, the favorable specific interactions between the polymer and the solvent can be observed. The weight fraction activity coefficient OMEGA1 infinity and the Flory-Huggins interaction parameter chi12infinity at infinite dilution and the effective exchange interation parameter chi12BAR of the system were calculated. These values confirm that the tert-butyl acetate is a poor solvent for this polymer, at 160-degrees-C. | en |
| dc.identifier.endpage | 172 | |
| dc.identifier.issn | 1060-1325 | |
| dc.identifier.startpage | 167 | |
| dc.identifier.uri | https://hdl.handle.net/20.500.14981/47975 | |
| dc.identifier.volume | A30 | |
| dc.identifier.wos | A1993KC28300020 | |
| dc.language.iso | eng | |
| dc.publisher | MARCEL DEKKER INC | |
| dc.relation.ispartof | JOURNAL OF MACROMOLECULAR SCIENCE-PURE AND APPLIED CHEMISTRY | |
| dc.subject | Polymer Science | |
| dc.title | THE RETENTION DIAGRAM OF POLY(P-CHLOROSTYRENE) AND TERT-BUTYL ACETATE BY THE INVERSE GAS-CHROMATOGRAPHY METHOD | |
| dc.type | Article | |
| dspace.entity.type | Publication | |
| local.import.source | WOS |