Yayın:
Swelling Characterization of the Superabsorbent Copolymer in the Petroleum-Based Solvent-Water Mixtures

dc.contributor.authorIsmail, Osman
dc.contributor.authorBeyribey, Berceste
dc.contributor.institutionauthorİSMAİL, Osman
dc.date.accessioned2026-06-27T13:16:53Z
dc.date.issued2012
dc.description.abstractThe crosslinked and porous copolymer grains were synthesized by inverse suspension polymerization of acrylamide. The synthesized copolymer was characterized by Fourier Transform Infrared Spectroscopy (FTIR) and Scanning Electron Microscopy (SEM). It was achieved to absorbed 418 g water by 1 g copolymer after 5 min waiting time. Moreover, it was seen that about 99% of water was absorbed by 1 g copolymer in the solvent water mixtures (300 mL solvent-200 mL distilled water) after 2.5 min waiting time. The diffusion coefficients of the copolymer in the solvent-water mixtures were found between 8.87.10(4) and 10.64.10(4) cm(2)s(-1). Furthermore, the copolymer in distilled water achieved to reach a high value of the diffusion coefficient (13.2.10(4) cm(2)s(-1)).en
dc.description.urihttps://doi.org/10.1080/10601325.2012.672052
dc.identifier.doi10.1080/10601325.2012.672052
dc.identifier.endpage438
dc.identifier.issn1060-1325
dc.identifier.issue5
dc.identifier.startpage432
dc.identifier.urihttps://hdl.handle.net/20.500.14981/51410
dc.identifier.volume49
dc.identifier.wos000303213800008
dc.language.isoeng
dc.publisherTAYLOR & FRANCIS INC
dc.relation.ispartofJOURNAL OF MACROMOLECULAR SCIENCE PART A-PURE AND APPLIED CHEMISTRY
dc.subjectSwelling
dc.subjectsuperabsorbent polymer
dc.subjectdiffusion
dc.subjectwater absorption
dc.subjectsolvent-water mixtures
dc.subjectHYDROGELS
dc.subjectTRANSPORT
dc.subjectRELEASE
dc.subjectPolymer Science
dc.titleSwelling Characterization of the Superabsorbent Copolymer in the Petroleum-Based Solvent-Water Mixtures