| dc.date.issued | 2025 | |
| dc.description.abstract | This study addresses the urgent need for efficient self-healing methods in geopolymer mortars (GMs), which, with their favorable low-carbon character, are still vulnerable to microcracking and ongoing durability loss. GMs made of 50 % ceramic powder (CP) and 50% granulated blast furnace slag (GBFS), synthesized with sodium hydroxide (2-12 M) and sodium silicate (Na2SiO3/ NaOH = 1.0-2.0) at an initial sand-to-binder ratio of 2.5, were cured at temperatures of 40 degrees C to 100 degrees C. Artificial microcracks with diameters of 0.2 mm and 0.6 mm were created before applying liquid (+S) and gel-like (+J) formulations of S. pasteurii and marine actinomycetes isolated from Marmara Sea sediments for 90-day treatments. Compressive and flexural strength, water absorption, ultrasonic pulse velocity (UPV), and microstructural analyses via SEM/EDS, XRD, and FTIR were considered methods for assessing healing performance. The S1 +S group showed the best mechanical recovery, with compressive and flexural strengths of 42.92 MPa and 8.98 MPa, respectively, while S26 +S showed the best UPV value of 3245.44 m/s, attesting to effective internal consolidation. S13 +S showed the most balanced improvement in acetate-decomposing strains, with compressive strength of 37.20 MPa, flexural strength of 5.63 MPa, and minimized water absorption (7.44 %). Preservation of calcite precipitation and crystalline geopolymeric phases were confirmed via XRD. At the same time, increased carbonate and Si-O-Al bonding in FTIR indicated that the microbe-induced and inorganic polymerized structures occurred simultaneously. EDS also supported these findings, where increased Ca and C contents asserted localized CaCO3 accumulation and increased peaks for Si and Al confirmed the unstable geopolymerization. All these findings place marine actinomycetes-especially acetate-decomposing strains-at the forefront of prospects for self-sustaining crack healing and structural reinforcement in green GMs. | en |
| dc.description.uri | https://doi.org/10.1016/j.cscm.2025.e04954 | |
| dc.identifier.doi | 10.1016/j.cscm.2025.e04954 | |
| dc.identifier.issn | 2214-5095 | |
| dc.identifier.uri | https://hdl.handle.net/20.500.14981/70117 | |
| dc.identifier.volume | 23 | |
| dc.identifier.wos | 001525909800001 | |
| dc.language.iso | eng | |
| dc.publisher | ELSEVIER | |
| dc.relation.ispartof | CASE STUDIES IN CONSTRUCTION MATERIALS | |
| dc.rights | openAccess | |
| dc.subject | Bio-activated geopolymer mortars | |
| dc.subject | Waste ceramic powder | |
| dc.subject | Microbial calcium carbonate precipitation | |
| dc.subject | Marine actinomycete | |
| dc.subject | BACTERIA | |
| dc.subject | Construction & Building Technology | |
| dc.subject | Engineering | |
| dc.subject | Materials Science | |
| dc.title | Innovative gel method: Sustainable crack healing in ceramic powder geopolymer mortars via marine actinomycetes and bioactivated carriers | |
| dc.type | Article | |
| dspace.entity.type | Publication | |
| local.import.source | WOS |