Yayın:
Optimization of leaching conditions for extraction of magnesium from a chromite beneficiation plant tailing predominantly containing lizardite

dc.contributor.authorCiftci, Hakan
dc.contributor.authorArslan, Bekir
dc.contributor.authorBilen, Aysegul
dc.contributor.authorArsoy, Zeyni
dc.contributor.authorErsoy, Bahri
dc.date.accessioned2026-06-27T14:32:48Z
dc.date.issued2021
dc.description.abstractIn this study, leaching experiments were performed for extraction of magnesium from a chromite beneficiation plant tailing predominantly containing lizardite. The X-ray fluorescence (XRF) and X-ray diffraction (XRD) analyzes showed that the tailing sample contains 39.3wt.% MgO and consist of predominantly lizardite mineral. Hydrochloric acid (HCl) and sulphuric acid (H2SO4) were used as acids separately in leaching experiments. Acid concentration, leaching temperature, leaching time, and solid ratio were investigated as leaching parameters and optimized. Maximum magnesium extraction yield was determined to be nearly 98% for both acids under optimum leaching parameters which leaching temperature was 85 degrees C, solid ratio was 20wt.%, leaching time was 120 minutes, and acid concentrations were 6 M for HCl and 4 M for H2SO4. In addition, it was determined that the leaching residue as a solid state was mainly composed of amorphous silicate according to the XRD analysis. Dissolution rate data were explained using Jander equation. Mg dissolution process found to be diffusion controlled.en
dc.description.urihttps://doi.org/10.19111/bulletinofmre.827630
dc.identifier.doi10.19111/bulletinofmre.827630
dc.identifier.endpage259
dc.identifier.issn0026-4563
dc.identifier.startpage251
dc.identifier.urihttps://hdl.handle.net/20.500.14981/61899
dc.identifier.volume164
dc.identifier.wos000644468700012
dc.language.isoeng
dc.publisherMADEN TETKIK VE ARAMA GENEL MUDURLUGU-MTA
dc.relation.ispartofBULLETIN OF THE MINERAL RESEARCH AND EXPLORATION
dc.rightsopenAccess
dc.subjectLeaching
dc.subjectLizardite
dc.subjectMagnesium
dc.subjectAmorphous silicate
dc.subjectChromite plant tailing
dc.subjectCARBON CAPTURE
dc.subjectDISSOLUTION KINETICS
dc.subjectSERPENTINE
dc.subjectCHRYSOTILE
dc.subjectSTORAGE
dc.subjectSILICA
dc.subjectPH
dc.subjectMINERALIZATION
dc.subjectPRECIPITATION
dc.subjectFIXATION
dc.subjectGeology
dc.titleOptimization of leaching conditions for extraction of magnesium from a chromite beneficiation plant tailing predominantly containing lizardite
dc.typeArticle