dc.description.abstractSi3N4/C composites were prepared with carbon black and alpha-Si3N4 powder by a novel sintering method, i. e. spark plasma sintering. SiC particles formed through reactions between the carbon particles and the SiO2 on the Si3N4 surface. The samples were sintered at 1650 degrees C for 5 minutes in a nitrogen atmosphere. The microstructure, phase composition, mechanical properties, and dielectric properties of the composites were investigated. The relative densities of the C/Si3N4 composites decreased from 99 to 85 % when the carbon black content increased from 0 to 20 wt.-%. Bending strength, hardness and dielectric properties were found to be influenced by the amount of carbon black introduced into the silicon nitride matrix.en
dc.description.sponsorshipScientific Research Foundation of the Yildiz Technical University
dc.description.urihttps://doi.org/10.3139/120.110138
dc.identifier.doi10.3139/120.110138
dc.identifier.endpage378
dc.identifier.issn0025-5300
dc.identifier.issue6
dc.identifier.startpage374
dc.identifier.urihttps://hdl.handle.net/20.500.14981/47625
dc.identifier.volume52
dc.identifier.wos000280049200006
dc.language.isoeng
dc.publisherCARL HANSER VERLAG
dc.relation.ispartofMATERIALS TESTING
dc.subjectCERAMICS
dc.subjectSILICON
dc.subjectMaterials Science
dc.titleSpark Plasma Sintering of Si3N4/C Composites
dc.typeArticle
dspace.entity.typePublication
local.import.sourceWOS

Dosyalar

Koleksiyonlar